$92.00 D14.4/D14.4M:2012 SPECIFICATION FOR WELDED JOINTS IN MACHINERY AND EQUIPMENT

(2012)

This specification establishes common acceptance criteria for classifying and applying carbon and low-alloy steel welded joints used in the manufacture of machines and equipment.

It also covers weld joint design, workmanship, quality control requirements and procedures, welding operator and welding procedure qualification, weld joint inspection (visual, radiographic, ultrasonic, magnetic particle, liquid penetrant), repair of weld defects, and heat treatment.

122 pages, 16 Tables, 38 Figures.