$72.00 D9.1M/D9.1:2012 SHEET METAL WELDING CODE

(2012)

Covers arc and braze welding requirements for nonstructural sheet metal fabrications using commonly welded metals available in sheet form up to and including 3 gauge, or 6.07 mm (0.239 in.). Applications of the code include heating, ventilating, and air conditioning systems, food processing equipment, architectural sheet metal, and other nonstructural sheet metal applications.

Sections include procedure and performance qualification, workmanship, and inspection. Nonmandatory annexes provide useful information on materials and processes. Not applicable when negative or positive pressure exceeds 30 kPa (5 psi). 70 pages, 29 figures, 10 tables, (2006).