$248.00 B2.1-8-215: 2001 STANDARD WELDING PROCEDURE SPECIFICATION(WPS) FOR; GAS TUNGSTEN ARC WELDING WITH CONSUMABLE INSERT OF AUSTENITIC STAINLESS STEEL (M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, IN3XX AND ER3XX, AS-WELDED CONDITION(PRIMARILY PIPE

(2001)

This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 through 1-1/2 inch, using manual gas tungsten arc welding with consumable insert root. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for groove welds. This WPS was developed primarily for pipe applications. ISBN 0-87171-697-6