WHB-1.9 WELDING HANDBOOK VOLUME 1 - WELDING SCIENCE & TECHNOLOGY (AWS WHB-1.9) (BACKORDER)
(2001)
Presents the latest developments in the basic science and technology of welding, and general descriptions of processes, continues with chapters on the physics of welding and cutting; heat flow; welding metallurgy; design; test methods; residual stress; welding symbols; tooling and positioning; monitoring and control; mechanized, automated, and robot ic techniques; economics; weld quality; inspection; qualification and certification; welding codes and standards; and safe practices.
932 pages, 17 chapters, 2 appendices, 530 illustrations, 168 tables, hardbound. 8" x 10", (2001).
ISBN 0-87171-657-7 ISBN 0-87171-657-7