$248.00 B2.1-1-234: 2006 (SWPS) FOR ARGON PLUS 25% CARBON DIOXIDE SHIELDED FLUX CORED ARC WELDING OF CARBON STEELl (M-1/P-1/S-1, GROUPS 1 and 2), 1/8 THROUGH 1-1/2 INCH THICK, E7XT-X, AS-WELDED OR PWHT CONDITION

(2006)

This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using Argon plus 25% CO2 shielded flux cored arc welding. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for groove and fillet welds. This WPS was developed primarily for pipe applications. ISBN 0-87171-017-X