$64.00 G2.4/G2.4M:2007 GUIDE FOR THE FUSION WELDING OF TITANIUM AND TITANIUM ALLOYS

(2007)

The standard Guide for the Fusion Welding of Titanium and Titanium Alloys provides instructional guidance for the welding of titanium and titanium alloys. This guide explains processes, equipment, materials, workshop practices, joint preparation, welding technique, tests, and the repair of defects. ISBN 0-87171-055-2