B1.10: 1999 GUIDE FOR THE NONDESTRUCTIVE EXAMINATION OF WELDS (HISTORICAL)
(1999)
This guide acquaints the user with the nondestructive examination methods commonly used the examine weldments. The standard also addresses which method best detects various types of discontinuities The examination methods included are visual, penetrant, magnetic, radiographic, ultrasonic, electromagnetic (eddy current), and leak testing. ISBN 0-87171-609-7