$248.00 B2.1-1-003:2002 (R2013) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR; GAS METAL ARCWELDING (SHORT CIRCUITING TRANSFER MODE) OF GALVANIZED STEEL (M-1), 18 THROUGH 10 GAUGE, IN THE AS-WELDED CONDITION, WITH OR WITHOUT BACKING

(2013)

This standard contains the essential welding variables for welding galvanized steel in the thickness range of 18 through 10 gauge, using semiautomatic gas metal arc welding (short circuiting transfer mode). It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for groove welds and fillet welds. ISBN 0-87171-675-5