B2.1-1-020: 1994-AMD1 STANDARD WELDING PROCEDURE SPECIFICATION(WPS) FOR; 75% AR/25% CO2 SHIELDED FLUX CORED ARC WELDING OF CARBON STEEL(M-1/P-1/S-1, GROUP1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, E70T-1 AND E71T-1, AS-WELDED OR PWHT CONDITION
(1994)
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using semiautomatic Ar/CO2 shielded flux cored arc welding. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for fillet and groove welds. This WPS was developed primarily for plate and structural applications. ISBN 0-87171-429-9