D1.1/D1.1M: 2008 STRUCTURAL WELDING CODE-STEEL (WITH 2009 ERRATA) (HISTORICAL)
(2008)
This code covers the welding requirements for any type of welded structure made from the commonly used carbon and low-alloy constructional steels. Clauses 1 through 8 constitute a body of rules for the regulation of welding in steel construction. There are eight normative and twelve informative annexes in this code. A Commentary of the code is included with the document. ISBN 978-0-87171-090-1