$248.00 B2.1-1-204: 1996(R2007) (SWPS) FOR; SHIELDED METAL ARC WELDING OF CARBON STEEL(M-1/P-1/S-1, GROUP 1 OR 2), 1/8THROUGH3/4 INCH THICK, E6010(VERTICAL DOWNHILL ROOT WITH THE BALANCE VER-TICAL UPHILL), AS-WELDED CONDITIO

(1996(R2007))

This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 3/4 inch, using manual shielded metal arc welding with E6010 (vertical downhill root with the balance vertical uphill). It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for fillet and groove welds. This WPS was developed primarily for pipe applications. ISBN 0-87171-491-4