$248.00 B2.1-1/8-014:2002 (R2013) (SWPS) FOR SHEILDED METAL ARC WELDING OF CARBON STEEL TO AUSTENITIC STAINLESS STEEL (M-1 TO M-8/P-8/S-8, GROUP 1), 10 THROUGH 18 GAUGE, IN THE AS-WELDED CONDITION, WITH OR WITHOUT BACKING; SITE LICE

(2013)

This standard contains the essential welding variables for welding carbon steel to austenitic stainless steel in the thickness range of 10 through 18 gauge using manual shielded metal arc welding. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for fillet welds and groove welds. ISBN 0-87171-686-0