The standard Guide for the Fusion Welding of Zirconium and Zirconium Alloys provides instructional guidance for the welding of zirconium and zirconium alloys. ISBN: 978-0-87171-802-0
This guide explains:
- processes
- equipment
- materials
- workshop practices
- joint preparation
- welding techniques
- tests, and the repair of defects.