Picture of B2.1-8-214:2001(R2012) STANDARD WELDING PROCEDURE SPECIFICATION FOR GAS TUNGSTEN ARC WELDING FOLLOWED BY SHIELDED METAL ARC WELDING OF AUSTENITIC STAINLESS STEEL, (M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, ER3XX AND E3XX-XX, AS-WELDED CONDITION

B2.1-8-214:2001(R2012) STANDARD WELDING PROCEDURE SPECIFICATION FOR GAS TUNGSTEN ARC WELDING FOLLOWED BY SHIELDED METAL ARC WELDING OF AUSTENITIC STAINLESS STEEL, (M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, ER3XX AND E3XX-XX, AS-WELDED CONDITION



Member Price: $204.00

Non-Member Price: $272.00

This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 through 1-1/2 inch, using manual gas tungsten arc welding followed by shielded metal arc welding. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for fillet and groove welds. This WPS was developed primarily for pipe applications.

Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$204.00
$272.00
Download PDF
$204.00
$272.00