A5.1/A5.1M:2012 SPECIFICATION FOR CARBON STEEL ELECTRODES

ERRATA FOR THIS CODE PROVIDED, CLICK HERE



Member Price: $54.00

Non-Member Price: $72.00

This specification establishes the requirements for classification of carbon steel electrodes for shielded metal arc welding. The requirements include mechanical properties of weld metal, weld metal soundness, and usability of electrode. Requirements for composition of the weld metal, moisture content of low-hydrogen electrode coverings, standard sizes and lengths, marking, manufacturing, and packaging are also included. A guide to the use of the standard is included in an annex.

Optional supplemental requirements include improved toughness and ductility, lower moisture contents, and diffusible hydrogen limits.

This specification makes use of both U.S. Customary Units and the International System of Units (SI). Since these are not equivalent, each system must be used independently of the other.

Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$54.00
$72.00
Download PDF
$54.00
$72.00