Provides guidance on visual examination of welds, including sections on prerequisites, fundamentals, surface conditions, and equipment. Sketches and color photographs illustrate common weld discontinuities. 42 pages, 3 annexes, 48

figures (2015) ISBN 978-0-87171-858-7