Picture of AASHTO/AWS D1.5M/D1.5:2015-AMD1 BRIDGE WELDING CODE

AASHTO/AWS D1.5M/D1.5:2015-AMD1 BRIDGE WELDING CODE



Member Price: $300.00

Non-Member Price: $400.00

This code covers the welding requirements for AASHTO welded highway bridges made from carbon and low-alloy constructional steels. This 2015 edition contains dimensions in metric SI Units and U.S. Customary Units. Clauses 1 through 7 constitute a body of rules for the regulation of welding in steel construction. The provisions for Clause 9 have been distributed throughout the D1.5 code. Clauses 8, 10, and 11 do not contain provisions, as their analogue D1.1 sections are not applicable to the D1.5 code. Clause 12 contains the requirements for fabricating fracture critical members.




AMENDMENT FOR THIS CODE PROVIDED, CLICK HERE

Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$300.00
$400.00
Download PDF
$300.00
$400.00