C2.21M/C2.21:2015 SPECIFICATION FOR THERMAL SPRAY EQUIPMENT ACCEPTANCE INSPECTION
Member Price: $56.00
Non-Member Price: $74.00
This standard specifies the essential elements of a procedure for verifying the performance of thermal spray equipment to ensure it is capable of operating according to the manufacturer’s specifications or those established by the User. ISBN: 978-0-87171-873-0