Picture of B4.0:2016 STANDARD METHODS FOR MECHANICAL TESTING OF WELDS

B4.0:2016 STANDARD METHODS FOR MECHANICAL TESTING OF WELDS



Member Price: $96.00

Non-Member Price: $128.00

Mechanical test methods that are applicable to welds and welded joints are described. For each testing method, information is provided concerning applicable American National Standards Institute (ANSI), American Society for Testing and Materials (ASTM), and American Petroleum Institute (API) documents; the required testing apparatus, specimen preparation, procedure to be followed, and report requirements are also described. ISBN: 978-0-87171-889-1