This chapter addresses the design of welded connections and the process of devising a welded connection that can transmit loads between two or more members. The primary focus of this chapter is on the performance of the welded connection in service. Design, or more specifically “engineering design,” is defined by ABET as “the process of devising a system, component, or process to meet desired needs.”4 A “connection” is defined as “combination of structural elements and joints used to transmit loads between two or more members.