This standard describes the test methods used to obtain brazed strength data of the short-time testing of single-lap joints in shear, butt-tension, stress-rupture, creep-strength, four-point-bending, and ceramic-tensile-button specimens. Specimen preparation methods, brazing procedures, testing techniques, and methods for data analysis are detailed. Sample forms for recording data are presented. A graphical method of data presentation relates shear stress to overlap distance. ISBN 978-0-87171-086-4