Picture of D17.3/D17.3:2021 SPECIFICATION FOR FRICTION STIR WELDING OF ALUMINUM ALLOYS FOR AEROSPACE APPLICATIONS

D17.3/D17.3:2021 SPECIFICATION FOR FRICTION STIR WELDING OF ALUMINUM ALLOYS FOR AEROSPACE APPLICATIONS



Member Price: $68.00

Non-Member Price: $90.00

This specification covers the general requirements for the friction stir welding of aluminum alloys for aerospace applications. It includes the requirements for weldment design, qualification of personnel and procedures, fabrication, and inspection. ISBN Print: 978-1-64322-151-9 ISBN PDF: 978-1-64322-152-6