C3.2M/C3.2:2008 STANDARD METHOD FOR EVALUATING THE STRENGTH OF BRAZED JOINTS

Member Price: $54.00

Non-Member Price: $72.00

This standard describes the test methods used to obtain brazed strength data of the short-time testing of single-lap joints in shear, butt-tension, stress-rupture, creep-strength, four-point-bending, and ceramic-tensile-button specimens. Specimen preparation methods, brazing procedures, testing techniques, and methods for data analysis are detailed. Sample forms for recording data are presented. A graphical method of data presentation relates shear stress to overlap distance. ISBN 978-0-87171-086-4





Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$54.00
$72.00
Download PDF
$54.00
$72.00