B2.1-1-018:1994R2005 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SELF-SHIELDED FLUX CORED ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2),1/8 THROUGH 1-1/2 INCH THICK, E71T-8, AS-WELDED CONDITION



Member Price: $204.00

Non-Member Price: $272.00

This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using semiautomatic self-shielded flux cored arc welding. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for fillet and groove welds. This WPS was developed primarily for plate and structural applications. ISBN 0-87171-427-2 

 