Alphabetical glossary of over 1,400 standard terms and definitions for welding, brazing, soldering, resistance welding, etc., as well as hybrid processes. Each term has one clearly applicable definition, accurately reflecting the term’s use in the joining world. Includes figures to illustrate the use of terms. For completeness, nonstandard terms are also included. Contains a Master Chart of Welding and Allied Processes, an d the Joining Method Chart. 160 pages, 62 figures, 5 tables (2010). ISBN: 978-0-87171-763-4