Picture of SWR-1 5 PIECE SET REPLICA WELDING SET

SWR-1 5 PIECE SET REPLICA WELDING SET



Member Price: $365.00

Non-Member Price: $365.00

The five-piece set is designed for training structural welding inspectors and welders. The samples include: 2 fillet-welded lap joints; 4-piece bend sample set; groove-welded butt joint. The variety of discontinuities exhibited includes: undercut, overlap and porosity. In addition, measurements of reinforcement and fillet weld size can be readily made.

It is recommended for those preparing for the Practical (Hands-on) portion of the AWS Certified Welding Inspector examination. It is also excellent for other weld examination training programs requiring hands-one experience.

T-joint Porosity Sample:
Side A: Location A1: Cluster Porosity: (1/8”)+(3x3/23)=13/32 (0.406”)
Location A2: Random Porosity: (3x1/8”)=3/8” (0.375”)
Location A3: Random Porosity: (1/8”)+3x1/16”)=5/16 (0.313”) Weld size = ¼”
Side B: Location B1: Linear Porosity: (2x1/16”)+(2x3/32”)=5/16” (0.313”).
Location B2: Random Porosity: (1/8”)+(2x3/32”)+(2x1/16”)=7/16” (0.438”)
Location B3: Random Porosity: (1/8”)+(2x3/32”)+(2x1/16”)=7/16” (0.438”)
Weld size = ½”

Butt Joint Sample:
Undercut greater than 1/32”
Weld reinforcement greater than 1/32” and less than 1/8”

Guided Bend Samples:
Bend A: Acceptable corner crack (3/16”), Rejectable crack (5/32”)
Bend B: Acceptable porosity (2@1/16”)
Bend C: Acceptable crack (5/64”), Rejectable crack (9/64”)
Bend D: No discontinuities

Fillet Weld Sample A:
Side 1: Overlap present
Pockmark less than 3/8”, 2-1/2” from left end
Weld size = 3/16”
Side 2: Weld size = 3/16”
Side 3: Acceptable porosity
Weld size = ¼”
Side 4: Undercut less than 3/32”
Weld size = 3/16”

Filet Weld Sample B:
Side 1: Pockmark less than 7?8”, 2-1/2” from left end
Weld size = ¼”
Side 2: Multi-pass.
Weld size = 5/16”
Side 3: Arc strike 1-3/4” from left end
Weld size = 3/16”
Side 4: Pockmark greater than 5/8 (0.688), 1-1/4” from left end