  • AWS-NAVSEA B2.1-1-301:2018

    Department: Technical
    Formats: Printed Hard Copy, Download PDF

    Member Price: $204.00 Non-Member Price: $272.00

    This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using manual gas tungsten arc weldi...

    Read More

     
  • AWS-NAVSEA B2.1-1-311:2018

    Department: Technical
    Formats: Printed Hard Copy, Download PDF

    Member Price: $204.00 Non-Member Price: $272.00

    This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using manual gas tungsten arc weldi...

    Read More

     
  • AWS-NAVSEA B2.1-8-309:2018

    Department: Technical
    Formats: Printed Hard Copy, Download PDF

    Member Price: $204.00 Non-Member Price: $272.00

    This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using manual shielded...

    Read More

     
  • AWS-NAVSEA B2.1-8-319:2018

    Department: Technical
    Formats: Printed Hard Copy, Download PDF

    Member Price: $204.00 Non-Member Price: $272.00

    This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using manual shielded...

    Read More

     
  • B2.1-8-308:2016

    Department: Technical
    Formats: Printed Hard Copy, Download PDF

    Member Price: $204.00 Non-Member Price: $272.00

    Standard Welding Procedure Specification for Naval Applications (SWPS-N) for Gas Tungsten Arc Welding of Austenitic Stainless Steel (S-8), 1/8 inch [3 mm] through 1-1/2 inch [38 mm] Thick, MIL-3XX, in the As-Welded Condition, Primarily Plate and Structural Naval Applications

    This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using manual gas tu...

    Read More

     
  • B2.1-8-318:2016

    Department: Technical
    Formats: Printed Hard Copy, Download PDF

    Member Price: $204.00 Non-Member Price: $272.00

    Standard Welding Procedure Specification for Naval Applications (SWPS-N) for Gas Tungsten Arc Welding of Austenitic Stainless Steel (S-8), 1/8 inch [3 mm] through 1-1/2 inch [38 mm] Thick, MIL-3XX, in the As-Welded Condition, Primarily Pipe for Naval Applications

    This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using manual gas tu...