  • B2.1-1-016:1994R2005 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHIELDED METAL ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 or 2), 1/8 THROUGH 1-1/2 INCH THICK, E7018, AS-WELDED OR PWHT CONDITION (HISTORICAL)

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using manual shielded metal arc welding. It cites the base...

    Read More

     
  • IS0 13919-1:1996(E)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $102.00 Non-Member Price: $136.00

    Welding - Electron and laser-beam welded joints - Guidance on quality levels for imperfections - Part 1: Steel

    Read More

     
  • A5.20:1995 CARBON STEEL ELECTRODES FOR FLUX CORED ARC WELDING (HISTORICAL)

    Member Price: $92.00 Non-Member Price: $92.00

    NOTE: THIS IS A 1995 HISTORICAL VERSION OF THE A5.20
    This specification prescribes the requirements for classification of carbon steel electrodes for flux cored...

    Read More

     
  • B2.1-1-017:1994 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHIELDED METAL ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, E6010, AS-WELDED OR PWHT CONDITION

    Formats: Printed Hard Copy, Download PDF

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using manual shielded metal arc welding. It cites the base...

    Read More

     
  • B2.1-1-018:1994R2005 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SELF-SHIELDED FLUX CORED ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2),1/8 THROUGH 1-1/2 INCH THICK, E71T-8, AS-WELDED CONDITION (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using semiautomatic self-shielded flux cored arc weldin...

    Read More

     
  • B2.1-1-019:1994-AMD1 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR CO2 SHIELDED LUX CORED ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, E70T-1 AND E71T-1, AS-WELDED CONDITION (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using semiautomatic CO2 shielded flux cored arc welding. I...

    Read More

     
  • B2.1-1-020:1994-AMD1 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR 75% AR/25% CO2 SHIELDED FLUX CORED ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, E70T-1 AND E71T-1, AS-WELDED OR PWHT CONDITION (HISTORICAL)

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using semiautomatic Ar/CO2 shielded flux cored arc welding...

    Read More

     
  • B2.1-1-021:1994R2005 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING FOLLOWED BY SHIELDED METAL ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, ER70S2 AND E7018, AS-WELDED OR PWHT CONDITION (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using manual gas tungsten arc welding followed by shielded...

    Read More

     
  • B2.1-1-026:1994 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHIELDED METAL ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, E6010(VERTICAL DOWNHILL) FOLLOWED BY E7018, AS-WELDED OR PWHT CONDITION (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using manual shielded metal arc welding. It cites the base...

    Read More

     
  • B2.1-8-023:1994 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHIELDED METAL ARC WELDING OF AUSTENITIC STAINLESS STEEL, (M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, AS-WELDED CONDITION (HISTORICAL)

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 through 1-1/2 inch, using manual shielded metal arc welding. It ...

    Read More