Railroads

Display per page
  • D15.3/D15.3M:2026 - SPECIFICATION FOR RESISTANCE WELDING FOR RAILROAD APPLICATIONS

    Formats: Printed Hard Copy, Download PDF

    Member Price: $78.00 Non-Member Price: $104.00

    This specification provides the general resistance welding requirements for railcars, locomotives, and their components. It includes, but is not limited to, resistance spot and res...

    Read More

     
  • D15.1/D15.1M:2025 - RAILROAD WELDING SPECIFICATION FOR CARS AND LOCOMOTIVES

    Formats: Printed Hard Copy, Download PDF

    Member Price: $165.00 Non-Member Price: $220.00

    This specification establishes minimum welding standards for the manufacture and maintenance of railcars, locomotives,
    and their components, intended for North American railro...

    Read More

     
  • D15.2/D15.2M:2022 SPECIFICATION FOR JOINING RAILROAD RAIL AND RELATED RAIL COMPONENTS

    Formats: Printed Hard Copy, Download PDF

    Member Price: $78.00 Non-Member Price: $104.00

    This document specifies the minimum standards for the welding of rails and related rail components. Repair procedures for rails and austenitic manganese steel components are covere...

    Read More

     
  • D15.1/D15.1M:2019 AMD1 RAILROAD WELDING SPECIFICATION FOR CARS AND LOCOMOTIVES (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $153.00 Non-Member Price: $204.00

    This specification establishes minimum welding standards for the manufacture and maintenance of railcars, locomotives, and their components, intended for North American railroad...

    Read More

     
  • D15.2/D15.2M:2013 RECOMMENDED PRACTICES FOR THE WELDING OF RAILS AND RELATED RAIL COMPONENTS FOR USE BY RAIL VEHICLES (HISTORICAL)

    Member Price: $72.00 Non-Member Price: $96.00

    This document recommends the minimum standards for the welding of rails and related rail components used by rail vehicles. Repair procedures for rails and austenitic manganese stee...

    Read More

     
...

...

...

...