Gas Tungsten Arc Welding
-
A5.7/A5.7M:2026 - SPECIFICATION FOR COPPER AND COPPER-ALLOY BARE WELDING RODS AND ELECTRODES
Formats: Printed Hard Copy, Download PDF
Member Price: $72.00 Non-Member Price: $96.00
This specification prescribes the requirements for classifications of copper and copper-alloy electrodes and rods for gas metal arc, gas tungsten arc, and plasma arc welding. Class... -
A5.22/A5.22M:2024 - SPECIFICATION FOR STAINLESS STEEL FLUX CORED AND METAL CORED WELDING ELECTRODES AND RODS
Formats: Printed Hard Copy, Download PDF
Member Price: $69.00 Non-Member Price: $92.00
Classification and other requirements are specified for numerous grades of flux cored and metal cored stainless steel electrodes and rods. New classifications include a duplex allo... -
A5.12M/A5.12:2024 (ISO 6848:2015 MOD) SPECIFICATION FOR TUNGSTEN AND OXIDE DISPERSED TUNGSTEN ELECTRODES FOR ARC WELDING AND CUTTING
Formats: Printed Hard Copy, Download PDF
Member Price: $110.00 Non-Member Price: $110.00
This specification prescribes the requirements for the classification of pure tungsten and oxide dispersed tungsten electrodes for gas tungsten arc welding and plasma arc welding a... -
B2.1-1-210:2023 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING WITH CONSUMABLE INSERTS OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, INMS-1 AND ER70S-2, AS-WELDED OR PWHT CONDITION
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 in [3 mm] through 1-1/2 in [38 mm], using manual gas tungsten arc welding w...
-
B2.1-1-211:2023 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING WITH CONSUMABLE INSERT ROOT FOLLOWED BY SHIELDED METAL ARC WELDING OF CARBON STEEL
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 in [3 mm] through 1-1/2 in [38 mm], using manual gas tungsten arc welding w...
-
B2.1-8-212:2023 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF AUSTENITIC STAINLESS STEEL (M-8/P-8, GROUP 1), 1/16 IN THROUGH 1-1/2 IN, ERXX, AS-WELDED CONDITION, PRIMARILY PIPE APLICATIONS
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/16 in [1.5 mm] through 1-1/2 in [38 mm], using manual gas tungs...
-
B2.1-8-214:2023 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING FOLLOWED BY SHIELDED METAL ARC WELDING OF AUSTENITIC STAINLESS STEEL (M-8/P-8, GROUP1), AS-WELDED CONDITION, PRIMARILY PIPE APPLICATIONS
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 in [1.5 mm] through 1-1/2 in [38 mm], using manual gas tungst...
-
B2.1-8-215:2023 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING WITH CONSUMABLE INSERT ROOT OF AUSTENITIC STAINLESS STEEL, 1/8IN THROUGH 1-1/2 IN THICK, IN3XX AND ER3XX, AS-WELDED CONDITION, PRIMARILY PIPE APPLICATIONS
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 in [3 mm] through 1-1/2 in [38 mm], using manual gas tungsten...
-
B2.1-8-216:2023 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING WITH CONSUMABLE INSERT ROOT FOLLOWED BY SHIELDED METAL ARC WELDING OF AUSTENITIC STAINLESS STEEL
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 in [3 mm] through 1-1/2 in [38 mm], using manual gas tungsten...
-
B2.1-8-024:2023 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF AUSTENITIC STAINLESS STEEL (M-8/P-8, GROUP 1), 1/16 IN THROUGH 1-1/2 IN THICK, ER3XX, AS-WELDED CONDITION PRIMARILY PLATE AND STRUCTURAL APPLICATIONS
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/16 in [1.5 mm] through 1-1/2 in [38 mm], using manual gas tungs...
Cart