B2.1-8-005:2002 (S2022) - STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS METAL ARC WELDING (SHORT CIRCUITING TRANSFER MODE) OF AUSTENITIC STAINLESS STEEL (M-8, P-8, OR S-8), 18 THROUGH 10 GAUGE, IN THE AS-WELDED CONDITION, WITH OR WITHOUT BACKING
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for welding austenitic stainless steel in the thickness range of 18 through 10 gauge, using semiautomatic gas metal a...
-
B2.1-1/8-006:2002 (S2022) - STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS METAL ARC WELDING (SHORT CIRCUITING TRANSFER MODE) OF CARBON STEEL TO AUSTENITIC STAINLESS STEEL (M-1 TO M-8, P-8, OR S-8), 18 THROUGH 10 GAUGE, WITH OR WITHOUT BACKING
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for welding carbon steel to austenitic stainless steel in the thickness range of 18 through 10 gauge, using semiautom...
-
B2.1-1-007:2002 (S2022) - STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF GALVANIZED STEEL (M-1),18 THROUGH 10 GAUGE, IN THE AS-WELDED CONDITION WITH OR WITHOUT BACKING
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for welding galvanized steel in the thickness range of 18 through 10 gauge using manual gas tungsten arc welding. Read More
-
B2.1-1-008:2002 (S2022) - STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF CARBON STEEL (M-1, P-1, OR S-1), 18 THROUGH 10 GAUGE, IN THE AS-WELDED CONDITION, WITH OR WITHOUT BACKING
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for welding carbon steel in the thickness range of 18 through 10 gauge using manual gas tungsten arc welding.
...
-
B2.1-8-009:2002 (S2022) - STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF AUSTENITIC STAINLESS STEEL (M-8, P-8, OR S-8), 18 THROUGH 10 GAUGE, IN THE AS-WELDED CONDITION, WITH OR WITHOUT BACKING
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for welding austenitic stainless steel in the thickness range of 18
through 10 gauge using manual gas tungsten arc weldi... -
B2.1-1-011:2002 (S2022) - STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHIELDED METAL ARC WELDING OF GALVANIZED STEEL (M-1), 10 THROUGH 18 GAUGE, IN THE AS-WELDED CONDITION, WITH OR WITHOUT BACKING
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for welding galvanized steel in the thickness range of 10 through
18 gauge, using manual shielded metal arc welding. It ... -
B2.1-1-012:2002 (S2022) - STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHIELDED METAL ARC WELDING OF CARBON STEEL, 10 THROUGH 18 GAUGE (M-1, P-1, OR S-1 TO M-1, P-1, OR S-1), IN THE AS-WELDED CONDITION, WITH OR WITHOUT BACKING
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for welding galvanized steel in the thickness range of 10 through
18 gauge, using manual shielded metal arc welding. It ... -
B2.1-8-013:2002 (S2022) - STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHIELDED METAL ARC WELDING OF AUSTENITIC STAINLESS STEEL (M-8/P-8/S-8, GROUP 1), 10 THROUGH 18 GAUGE, WITH OR WITHOUT BACKING
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for welding austenitic stainless steel in the thickness range of
18 through 10 gauge using manual shielded metal arc wel... -
B2.1-1/8-014:2002 (S2022) - STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHIELDED METAL ARC WELDING OF CARBON STEEL TO AUSTENITIC STAINLESS STEEL (M-1 TO M-8/P-8/S-8, GROUP 1), 10 THROUGH 18 GAUGE, WITH OR WITHOUT BACKING
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for welding carbon steel to austenitic stainless steel in the thickness
range of 10 through 18 gauge using manual shield... -
D15.2/D15.2M:2022 SPECIFICATION FOR JOINING RAILROAD RAIL AND RELATED RAIL COMPONENTS
Formats: Printed Hard Copy, Download PDF
Member Price: $78.00 Non-Member Price: $104.00
This document specifies the minimum standards for the welding of rails and related rail components. Repair procedures for rails and austenitic manganese steel components are covere...