Brazing and Braze Welding

Display per page
  • A5.31M/A5.31:2012 SPECIFICATION FOR FLUXES FOR BRAZING AND BRAZE WELDING (HISTORICAL)

    Member Price: $69.00 Non-Member Price: $92.00

    Eighteen fluxes for brazing and braze welding are classified according to the filler metal, form, and activity temperature range. Classification is in accordance with a classificat...

    Read More

     
  • ISO 13585:2012

    Member Price: $180.00 Non-Member Price: $180.00

    Brazing — Qualification test of brazers and brazing operators

    Read More

     
  • C3.7M/C3.7-2011 SPECIFICATION FOR ALUMINUM BRAZING (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $60.00 Non-Member Price: $80.00

    Addresses the minimum fabrication, equipment, material, process procedure requirements, and inspection requirements for aluminum brazing using the atmosphere furnace, vacuum furnac...

    Read More

     
  • C3.2M/C3.2:2008 STANDARD METHOD FOR EVALUATING THE STRENGTH OF BRAZED JOINTS (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $66.00 Non-Member Price: $88.00

    This standard describes the test methods used to obtain brazed strength data of the short-time testing of single-lap joints in shear, butt-tension, stress-rupture, creep-strength, ...

    Read More

     
  • BRH:2007 BRAZING HANDBOOK, 5th EDITION

    Formats: Printed Hard Copy, Download PDF

    Member Price: $138.00 Non-Member Price: $184.00

    Updated and expanded. Provides a comprehensive, organized survey of the basics of brazing, processes, and applications. Addresses the fundamentals of brazing, brazement design, bra...

    Read More

     
  • BHC1 - BASICS OF BRAZING

    Member Price: $30.00 Non-Member Price: $40.00

    Chapter 1 from the Brazing Handbook. Contents for this chapter include - Introduction, Historical Perspective, Physics of Brazing, Factors Controlling the Properties of the Brazeme...

    Read More

     
  • BHC2 - BRAZEMENT DESIGN

    Member Price: $30.00 Non-Member Price: $40.00

    Chapter 2 from the Brazing Handbook. Contents for this chapter include - Introduction, Design Variables, Base Metal, Joint Design, Fluxes and Protective Atmospheres, Stress Dist...

    Read More

     
  • BHC3 - BRAZING FILLER METALS

    Member Price: $30.00 Non-Member Price: $40.00

    Chapter 3 from the Brazing Handbook. Contents for this chapter include - Introduction, Melting of Brazing Metal-Base Metal Interaction, Brazing Filler Metal Selection, Brazing F...

    Read More

     
  • BHC4 - FLUXES AND ATMOSPHERES

    Member Price: $30.00 Non-Member Price: $40.00

    Chapter 4 from the Brazing Handbook. Contents for this chapter include - Introduction, Fluxes, Controlled Brazing Atmospheres, Bibliography, and Suggested Reading List.

    Read More

     
  • BHC5 - PRECLEANING AND SURFACE PREPARATION

    Member Price: $30.00 Non-Member Price: $40.00

    Chapter 5 from the Brazing Handbook. Contents for this chapter include - Introduction, Cleaning Processes, Surface Pretreatments, Braze Flow Inhibitors, Maintaining Cleanliness,...

    Read More

     
...

...

...

...