Carbon Steel
-
B2.1-1-012:2002(R2013) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHIELDED METAL ARC WELDING OF CARBON STEEL, (M-1, P-1, OR S-1 TO M-1, P-1, OR S-1), 10 THROUGH 18 GAUGE, IN THE AS-WELDED CONDITION, WITH OR WITHOUT BACKING (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for welding carbon steel in the thickness range of 10 through 18 gauge, using manual shielded metal arc welding. It cites the... -
B2.1-1/8-014:2002(R2013) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHEILDED METAL ARC WELDING OF CARBON STEEL TO AUSTENITIC STAINLESS STEEL, (M-1 TO M-8/P-8/S-8, GROUP 1), 10 THROUGH 18 GAUGE, IN THE AS-WELDED CONDITION, WITH OR WITHOUT BACKING (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for welding carbon steel to austenitic stainless steel in the thickness range of 10 through 18 gauge using manual shielded me... -
B2.1-1/8-227:2002 AMD1(R2013) STANDARD WELDING PROCEDURE SPECIFICATION FOR GTAW OF CARBON STEEL, (M-1/P-1/S-1, GROUPS 1 OR 2) TO AUSTENITIC STAINLESS STEEL (M-8/P-8/S-8, GROUP 1), 1/16 THROUGH 1-1/2 INCH THICK, ER309(L), AS-WELDED CONDITION (HISTORICAL)
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel to austenitic stainless steel in the thickness range of 1/16 through 1-1/2 inch, using manual gas tungsten a... -
B2.1-1/8-229:2002 AMD1(R2013) STANDARD WELDING PROCEDURE SPECIFICATION FOR GTAW FOLLOWED BY SHIELDED METAL ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUPS 1 OR 2) TO AUSTENITIC STAINLESS STEEL (M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for welding carbon steel to austenitic stainless steel in the thickness range of 1/8 through 1-1/2 inch, using manual gas tun... -
B2.1-1/8-230:2002 AMD1(R2013) STANDARD WELDING PROCEDURE SPECIFICATION FOR GTAW WITH CONSUMABLE INSERT ROOT OF CARBON STEEL, (M-1/P-1/S-1, GROUPS 1 OR 2) TO AUSTENITIC STAINLESS STEEL (M-8/P-8/S-8, GROUP 1), 1/16 THROUGH 1-1/2 INCH THICK (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for welding carbon steel to austenitic stainless steel in the thickness range of 1/16 through 1-1/2 inch, using manual gas tu... -
B2.1-1/8-228:2002(R2013) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SHIELDED METAL ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUPS 1 or 2) TO AUSTENITIC STAINLESS STEEL (M-8/ P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, E309(L)-15, -16, or -17 (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for welding carbon steel to austenitic stainless steel in the thickness range of 1/8 through 1-1/2 inch, using manual shielde... -
B2.1-1/8-006:2002(R2013) STANDARD WELDING PROCEDURE SPECIFICATION FOR GMAW (SHORT CIRCUITING TRANSFER MODE) OF CARBON STEEL TO AUSTENITIC STAINLESS STEEL, (M-1 TO M-8, P-8, OR S-8), 18 THROUGH 10 GAUGE, IN THE AS-WELDED CONDITION WITH OR WITHOUT BACKING (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for welding carbon steel to austenitic stainless steel in the thickness range of 18 through 10 gauge, using semiautomatic gas... -
B2.1-1-211:2001(R2012) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING WITH CONSUMABLE INSERT ROOT FOLLOWED BY SHIELDED METALARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUG1-1/2 INCH THICK, INMS-1, ER70S-2 (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using manual gas tungsten arc welding with consumable inse... -
B2.1-1-210:2001(R2012) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING WITH CONSUMABLE INSERTS OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, INMS-1 AND ER70S-2, AS-WELDED OR PWHT CONDITION (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using manual gas tungsten arc welding with consumable inse... -
A5.1/A5.1M:2012 SPECIFICATION FOR CARBON STEEL ELECTRODES (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $69.00 Non-Member Price: $92.00
This specification establishes the requirements for classification of carbon steel electrodes for shielded metal arc welding. The requirements include mechanical properties of weld...