Gas Metal Arc Welding

Display per page
  • B2.1-1-234:2006 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR ARGON PLUS 25% CARBON DIOXIDE SHIELDED FLUX CORED ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUPS 1 and 2), 1/8 THROUGH 1-1/2 INCH THICK, E7XT-X, AS-WELDED OR PWHT CONDITION (HISTORICAL)

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using Argon plus 25% CO2 shielded flux cored arc welding. ...

    Read More

     
  • B2.1-1-235:2006 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR ARGON PLUS 2% OXYGEN SHIELDED GAS METAL ARC WELDING (SPRAY TRANSFER MODE) OF CARBON STEEL (M-1/P-1/S-1, GROUPS 1 AND 2), 1/8 THROUGH 1-1/2 INCH THICK, ER70S-3, FLAT POSITION ONLY (HISTORICAL)

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using Argon plus 2% Oxygen shielded gas metal arc welding ...

    Read More

     
  • A5.24/A5.24M:2005 ZIRCONIUM AND ZIRCONIUM ALLOY WELDING ELECTRODES AND RODS (HISTORICAL)

    Member Price: $69.00 Non-Member Price: $92.00

    This specification prescribes the requirements for classification of zirconium and zirconium alloy electrodes and rods for GTA, GMA, and PA welding. AWS A5.24/A5.24M:2005 is a revi...

    Read More

     
  • B2.1-1-018:1994R2005 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR SELF-SHIELDED FLUX CORED ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2),1/8 THROUGH 1-1/2 INCH THICK, E71T-8, AS-WELDED CONDITION (HISTORICAL)

    Formats: Printed Hard Copy, Download PDF

    Member Price: $264.00 Non-Member Price: $352.00

    This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using semiautomatic self-shielded flux cored arc weldin...

    Read More

     
  • D2.0:1966 SPECIFICATIONS FOR WELDED HIGHWAY AND RAILWAY BRIDGES (HISTORICAL)

    Member Price: $90.00 Non-Member Price: $120.00

    D2.0:1966 SPECIFICATIONS FOR WELDED HIGHWAY AND RAILWAY BRIDGES AND AWS SRI-65 GAS METAL-ARC WELDING WITH CARBON DIOXIDE SHIELDING

    Read More

     
...

...

...

...