Gas Tungsten Arc Welding
-
B2.1-8-212:2001R(2012) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR; GAS TUNGSTEN ARC WELDING OF AUSTENITIC STAINLESS STEEL, (M-8/P-8/S-8, GROUP 1), 1/16 THROUGH 1-1/2 INCH THICK, ER3XX, AS-WELDED CONDITION (HISTORICAL)
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/16 through 1-1/2 inch, using manual gas tungsten arc welding. It c... -
B2.1-1-211:2001(R2012) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING WITH CONSUMABLE INSERT ROOT FOLLOWED BY SHIELDED METALARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUG1-1/2 INCH THICK, INMS-1, ER70S-2 (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using manual gas tungsten arc welding with consumable inse... -
B2.1-1-210:2001(R2012) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING WITH CONSUMABLE INSERTS OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, INMS-1 AND ER70S-2, AS-WELDED OR PWHT CONDITION (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 through 1-1/2 inch, using manual gas tungsten arc welding with consumable inse... -
B2.1-8-025:2001(R2012) STANDARD WELDING PROCEDURE SPECIFICATION FOR GAS TUNGSTEN ARC WELDING FOLLOWED BY SHIELDED METAL ARC WELDING OF AUSTENITIC STAINLESS STEEL, (M-8/P-8/S-8, GROUP 1), 1/8 THROUGH 1-1/2 INCH THICK, ER3XX AND E3XX-XX, AS-WELDED CONDITION (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 through 1-1/2 inch, using manual gas tungsten arc welding follow... -
B2.1-8-024:2001(R2012) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF AUSTENITIC STAINLESS STEEL, (M-8/P-8/S-8, GROUP 1), 1/16 THROUGH 1-1/2 INCH THICK, ER3XX, AS-WELDED CONDITION, PRIMARILY PLATE AND STRUCTURAL APPLICATIONS (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/16 through 1-1/2 inch, using manual gas tungsten arc welding. It c... -
B2.1-22-015:2011 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF ALUMINUM, (M/P/S-22 TO M/P/S-22), 18 THROUGH 10 GAUGE, IN THE AS-WELDED CONDITION, WITH OR WITHOUT BACKING (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for aluminum in the thickness range of 10 through 18 gauge using manual gas tungsten arc welding. It cites the base metals an... -
B2.1/B2.1M:2009 ADD1 SPECIFICATION FOR WELDING PROCEDURE AND PERFORMANCE QUALIFICATION (HISTORICAL)
Formats: Printed Hard Copy, Download PDF
Member Price: $210.00 Non-Member Price: $280.00
This specification provides the requirements for qualification of welding procedure specifications, welders, and welding operators for manual, semiautomatic, mechanized, and automa... -
B2.1-4-217:1999(R2009) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING OF CHROMIUM - MOLYBDENUM STEEL, (M-4/P-4, GROUP 1 or 2), ER80S-B2, 1/8 THROUGH 1/2 INCH THICK, AS-WELDED
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for chromium-molybdenum steel in the thickness range of 1/8 through 1/2 in. in the as-welded condition, or 1/8 through 3/4 in... -
B2.1-4-219:1999(R2009) STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING FOLLOWED BY SHIELDED METAL ARC WELDING OF CHROMIUM- MOLYBDENUM STEEL, (M-4/P-4, GROUP 1 OR 2), 1/8 THROUGH 1/2 INCH THICK
Formats: Printed Hard Copy, Download PDF
Member Price: $264.00 Non-Member Price: $352.00
This standard contains the essential welding variables for chromium-molybdenum steel in the thickness range of 1/8 through 1/2 in. in the as-welded condition, or 1/8 in. through 1-...