WHC4.06 CLAD AND DISSIMILAR METALS
Member Price: $24.00
Non-Member Price: $32.00
The information in this chapter addresses the fusion welding of clad and dissimilar metals. It does not address joining methods, such as brazing, in which there is insignificant alloying between the base metal and the added weld metal. The use or application of the techniques and guidelines presented in this chapter requires sufficient engineering, prefabrication testing, and fabrication controls to confirm in advance that the specific application requirements will be met by the completed product
If you want the entire hardcopy with all the chapters you can find it here
WHB-4.9 WELDING HANDBOOK VOLUME 4 - MATERIALS AND APPLICATIONS PART 1
You can also purchase electronic versions of each chapter. Click on any single chapter below to get the electronic version.