AWS C3.7M/C3.7-2011 SPECIFICATION FOR ALUMINUM BRAZING

Member Price: $48.00

Non-Member Price: $64.00

Addresses the minimum fabrication, equipment, material, process procedure requirements, and inspection requirements for aluminum brazing using the atmosphere furnace, vacuum furnace, and flux processes. ANSI Approved.