Picture of C7.1M/C7.1:2013 RECOMMENDED PRACTICES FOR ELECTRON BEAM WELDING AND ALLIED PROCESSES

C7.1M/C7.1:2013 RECOMMENDED PRACTICES FOR ELECTRON BEAM WELDING AND ALLIED PROCESSES



Member Price: $84.00

Non-Member Price: $112.00

Provides process definitions and requirements, safe practices, and inspection criteria for electron beam welding. Also covers common applications of electron beam welding. Includes numerous power curves for various alloys. ISBN 0-87171-721-2

Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$84.00
$112.00