C2.19/C2.19M:2013 SPECIFICATION FOR THE APPLICATION OF THERMAL SPRAY COATINGS TO MACHINE ELEMENTS FOR OEM AND REPAIR (HISTORICAL)



Member Price: $69.00

Non-Member Price: $92.00

This standard defines requirements for thermal spray coating systems for OEM and repair applications. Included are HVOF (High Velocity Oxygen Fuel) coatings that can be used as an alternative to hard chrome plating. The essential equipment, procedures for surface preparation, and the application of specific thermal spray coatings and sealers are detailed with in-process quality control checkpoints. This standard also presents management requirements and procedures for qualification, procedure approval, and documentation. Also covered are approved applications for thermal spray processes used for OEM and repair of machinery components along with minimum training requirements for thermal spray operators and inspectors. This specification has several annexes including annexes on safety, protocols for the U.S. Navy shipboard machinery, bend testing, and bond testing.

Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$69.00
$92.00
Download PDF
$69.00
$92.00