C3.2M/C3.2:2001 STANDARD METHOD FOR EVALUATING THE STRENGTH OF BRAZED JOINTS, INCLUDES 2-TABLES AND 12-FIGURES (HISTORICAL)
Member Price: $57.00
Non-Member Price: $76.00
A single-lap shear brazstandardized specimen was developed as the result of interlaboratory testing program. Additional test specimens have been added to obtain brazed strength data in butt tension, stress rupture, creep strength, and four-point bending. Specimen preparation methods, brazing procedures, testing techniques, and methods for data analysis are detailed. Sample forms for recording data are presented. A graphical method of data presentation relates shear stress to overlap distance.
Describes the test method used to obtain reliable data on the strength of brazed joints loaded in tensile, shear, and fourpoint bending. ANSI Approved. approx. 19 pages ISBN 0-87171-689-5