C4.4/C4.4M:2004 RECOMMENDED PRACTICES FOR HEAT SHAPING AND STRAIGHTENING WITH OXYFUEL GAS HEATING TORCHES (HISTORICAL)
Member Price: $52.00
Non-Member Price: $70.00
This document describes methods and techniques for shaping and straightening metal parts including steel plate, pipes, angles, channel, T bar, and compound structures by careful application of heat. It presents the theory and mathematical formulas for developing heat shaping patterns. Other topics include oxyfuel gas equipment torches, tips, regulators, fuel gases, gas cylinders, and bulk supply torch procedures for spot, line and v heating patterns, and safety procedures. Figures show the locations for placement of heating patterns to obtain desired results for straightening, forming, or bending operations. ANSI Approved. approx. 41 pages ISBN 0-87171-612-7