Picture of ISO 14323:2015(E)

ISO 14323:2015(E)



Member Price: $132.00

Non-Member Price: $132.00

Resistance welding — Destructive testing of welds — Specimen dimensions and procedure for impact tensile shear test and crosstension testing of resistance spot and embossed projection welds

Formats Member Price Non-Member Price Quantity
Download PDF
$132.00
$132.00