This standard lists and describes flaws and defects in hot gas, hot gas extrusion, heated tool butt fusion, socket fusion, electrofusion, and flow fusion welded joints in thermoplastics. Its intent is to make possible a generally valid evaluation giving consideration to graded quality requirements. This standard encompasses the classification, requirements, testing, evaluation, and acceptance of the welds. Details in recording engineering data are described. Tables illustrating cracks, voids, solid inclusions, lack of fusion, flaws and defects of shape, and other flaws and defects in thermoplastic welds are included. Flaw and defect features with descriptions and illustrations are compiled into tables to aid in the evaluation of welds. ISBN: 978-0-87171-884-6



Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$75.00
$100.00
Download PDF
$75.00
$100.00