D10.10/D10.10M:1999 RECOMMENDED PRACTICES FOR LOCAL HEATING OF WELDS IN PIPING AND TUBING (HISTORICAL)
Member Price: $70.00
Non-Member Price: $94.00
The current revision of this popular standard considers both local 360 band and spot heating thermocouple location, attachment and accuracy insulation provisions service environment and QA system considerations. It also contains a comparative analysis of radiant heating methods induction, electric resistance, flame, exothermic, gasflame generated infrared, quartz lamps. The AWS D10 Subcommittee on Local Heat Treating of Pipework states that, the objective of this document is to present recommended practices based on an ordered assessment of available research and information, rather than a summary of current practice. Offers sample Standard Procedure for Local Heating form. U.S. Customary and SI metric units. ANSI Approved. ISBN 0-87171-558-9