D10.18M/D10.18:2018 GUIDE FOR WELDING FERRITIC/AUSTENITIC DUPLEX STAINLESS STEEL PIPING AND TUBING
Member Price: $56.00
Non-Member Price: $74.00
This standard presents a detailed discussion of the metallurgical and welding characteristics and weldability of duplex stainless steel used in piping and tubing. A number of tables and graphs are presented in order to illustrate the text. ISBN: 978-0-87171-930-0