AWS-NAVSEA B2.1-1-304:2018 - Standard Welding Procedure Specification for Naval Applications (SWPS-N) for CO2 Shielded Flux Cored Arc Welding of Carbon Steel (S-1), 1/8" [3mm] through 1-1/2" [38mm] Thick, MIL-70T-1, MIL-71T-1, As-Welded Cond., Plate and Struc. Naval Apps.
Member Price: $264.00
Non-Member Price: $352.00
This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using semiautomatic carbon dioxide shielded flux cored arc welding. It cites the base metals and
operating conditions necessary to make the weldment, the filler metal specifications, and joint designs for groove and fil- let welds. This SWPS-N was developed primarily for naval applications that require performance to NAVSEA Technical
Publication S9074-AQ-GIB-010/248, Requirements for Welding and Brazing Procedure and Performance Qualification.