Picture of AWS-NAVSEA B2.1-1-317:2018 - Standard Welding Procedure Specification for Naval Applications for 75% Ar+25% CO2 Shielded Flux Cored Arc Welding of Carbon Steel (S-1), 1/8"[3 mm] --> 1-1/2"[38 mm] Thick, MIL-70T-1, MIL-71T-1, in As-Welded or PWHT Cond., Primarily Pipe for Naval Apps.

AWS-NAVSEA B2.1-1-317:2018 - Standard Welding Procedure Specification for Naval Applications for 75% Ar+25% CO2 Shielded Flux Cored Arc Welding of Carbon Steel (S-1), 1/8"[3 mm] --> 1-1/2"[38 mm] Thick, MIL-70T-1, MIL-71T-1, in As-Welded or PWHT Cond., Primarily Pipe for Naval Apps.



Member Price: $264.00

Non-Member Price: $352.00

This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using semiautomatic gas shielded flux cored arc welding. It cites the base metals and operating conditions
necessary to make the weldment, the filler metal specifications, and joint designs for groove and fillet welds. This SWPS-N was developed primarily for naval applications that require performance to NAVSEA Technical Publication S9074-AQ-GIB-010/248, Requirements for Welding and Brazing Procedure and Performance Qualification. ISBN: 978-0-87171-943-0

Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$264.00
$352.00
Download PDF
$264.00
$352.00