This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using semiautomatic CO2 shielded flux cored arc welding. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for fillet and groove welds. This SWPS was developed primarily for plate and structural applications. ISBN Print: 978-8-87171-959-1. ISBN PDF: 978-0-87171-960-7

Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$204.00
$272.00
Download PDF
$204.00
$272.00