Picture of AWS-NAVSEA B2.1-8-322:2018 - Standard Welding Procedure Specification for Naval Apps (SWPS-N) for GTAW w/Consumable Insert Root Followed by SMAW of Austenitic Stainless Steel (S-8), 1/8" through 1-1/2 " Thick, MIL-3XX, MIL-3XX-XX, in As-Welded Cond., Primarily Pipe for Naval Apps

AWS-NAVSEA B2.1-8-322:2018 - Standard Welding Procedure Specification for Naval Apps (SWPS-N) for GTAW w/Consumable Insert Root Followed by SMAW of Austenitic Stainless Steel (S-8), 1/8" through 1-1/2 " Thick, MIL-3XX, MIL-3XX-XX, in As-Welded Cond., Primarily Pipe for Naval Apps



Member Price: $264.00

Non-Member Price: $352.00

This standard contains the essential welding variables for austenitic stainless steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using manual gas tungsten arc welding with consumable insert root followed by shielded metal arc welding. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and joint designs for full penetration groove welds with consumable inserts. This SWPS-N was developed primarily for naval applications that require performance to NAVSEA Technical Publication S9074-AQGIB- 010/248, Requirements for Welding and Brazing Procedure and Performance Qualification. ISBN Print: 978-1-64322-012-3 ISBN PDF: 978-1-64322-013-0


Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$264.00
$352.00
Download PDF
$264.00
$352.00