Picture of B2.1-1-209:2019 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING FOLLOWED BY SHIELDED METAL ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, ER70S-2AND E7018, AS-WELDED OR PWHT CONDITION

B2.1-1-209:2019 STANDARD WELDING PROCEDURE SPECIFICATION (SWPS) FOR GAS TUNGSTEN ARC WELDING FOLLOWED BY SHIELDED METAL ARC WELDING OF CARBON STEEL, (M-1/P-1/S-1, GROUP 1 OR 2), 1/8 THROUGH 1-1/2 INCH THICK, ER70S-2AND E7018, AS-WELDED OR PWHT CONDITION



Member Price: $246.00

Non-Member Price: $328.00

This standard contains the essential welding variables for carbon steel in the thickness range of 1/8 inch [3 mm] through 1-1/2 inch [38 mm], using manual gas tungsten arc welding followed by shielded metal arc welding. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for fillet and groove welds. This SWPS was developed primarily for pipe applications. ISBN Print: 978-1-64322-048-2 ISBN PDF: 978-1-64322-049-9

Formats Member Price Non-Member Price Quantity
Printed Hard Copy
$246.00
$328.00
Download PDF
$246.00
$328.00